Bakin Karfe Flux Cored Waya EGT1-4 Reactor abubuwan walda
FASSARAR welding
Kar a bar tambayoyin
Ci gaba da ratsa ku
Rashin kwanciyar hankali
Gyaran mara kyau
Wuce kitse
Dace da walda SUS316Nb da 316Ti
Bugu da kari na Nb iya yadda ya kamata inganta juriya ga intergranular lalata
Ripple lafiya
Arc ɗin yana da taushi da kwanciyar hankali, ƙarancin fantsama, kyakkyawan tsari
Good slag kau, barga waya ciyar, tare da kyakkyawan aikin walda aiki.
Sauƙi slagging
Sigar Samfura
KASHIN KIMIYYA:
ALOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Sauran |
GB/T dokokin | 0.02 | 0.6 | 1.50 | 0.02 | 0.003 | 12 | 19.5 | 2.5 | Nb:0.25 |
DUKIYAR INJI:
DUKIYA | KARFIN KYAUTA (MPa) | KARFIN ARZIKI(MPa) | Tsawaita /% | IMAPACT DARAJAR J/℃ | Maganin zafi °C*h | |||||
GB/T dokokin | - | 650 | 35 | - | - |
SHAWARAR MATSALAR welding:
BAYANIN DIAMETERS(mm) | 1.2 | 1.6 | |||
Voltage (Volt) | 22-36 | 26-38 | |||
Wutar Lantarki (Amp) | 120-260 | 200-300 | |||
Gudun (mm/min) | 15-20 | 18-25 | |||
Tsawon tsayin bushewa (mm) | 15-25 | 15-25 |
Tallafin masana'anta
Samfurin ya dace da a
fadi da kewayon aikace-aikace
FASSARAR welding
Reactor na ciki
-
981 Semi-submersible drilling rig
-
8.2-ton babban mai ɗaukar kaya
KASHIN KIMIYYA:
ALOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Sauran |
GB/T dokokin | 0.02 | 0.6 | 1.50 | 0.02 | 0.003 | 12 | 19.5 | 2.5 | Nb:0.25 |
DUKIYAR INJI:
DUKIYA | KARFIN KYAUTA (MPa) | KARFIN ARZIKI(MPa) | Tsawaita /% | IMAPACT DARAJAR J/℃ | Maganin zafi °C*h | |||||
GB/T dokokin | - | 650 | 35 | - | - |
SHAWARAR MATSALAR welding:
BAYANIN DIAMETERS(mm) | 1.2 | 1.6 | |||
Voltage (Volt) | 22-36 | 26-38 | |||
Wutar Lantarki (Amp) | 120-260 | 200-300 | |||
Gudun (mm/min) | 15-20 | 18-25 | |||
Tsawon tsayin bushewa (mm) | 15-25 | 15-25 |